Hood, Second Coat of Body Filler

Next I applied a second coat of body filler to the areas of the hood that required it.
On the second coat I attempted to feather the filler out away from the dents to transition it into the undamaged areas of the hood. After the second coat dried I used my random orbital sander and a 120-grit sanding disk to sand it smooth.